LEAN DUPLEX STAINLESS STEELS—THE ROLE OF MOLYBDENUM IN PITTING CORROSION OF CONCRETE REINFORCEMENT STUDIED WITH INDUSTRIAL AND LABORATORY CASTINGS

LEAN  DUPLEX  STAINLESS  STEELS—THE  ROLE  OF  MOLYBDENUM  IN  PITTING  CORROSION  OF CONCRETE  REINFORCEMENT  STUDIED  WITH  INDUSTRIAL  AND  LABORATORY  CASTINGS

LEAN DUPLEX STAINLESS STEELS—THE ROLE OF MOLYBDENUM IN PITTING CORROSION OF CONCRETE REINFORCEMENT STUDIED WITH INDUSTRIAL AND LABORATORY CASTINGS

... low alloy duplex stainless steels (DSS) thường gọi thép lean duplex steel, làm tăng thêm tính đa dạng thép sử dụng gia cố bê tông Những loại DSS với thành phần Ni Mo thấp, tác động kinh tế thấp ... ăn mòn rỗ nhiều báo gần đây, Alvarez đồng nghiên cứu hoạt động ăn mòn hai loại tôn sóng lean duplex stainless steels (SAF 2001 2304) Thử nghiệm 2.1 Vật liệu Bốn DSS nạc khác với hai nồng độ khác ... hợp kim hiệu đóng vai trò quan trọng kháng ăn mòn rỗ DSS, người ta phải xem xét PREn biểu theo kinh nghiệm đề xuất từ danh mục kết thực nghiệm thu điều kiện cụ thể định, chủ yếu giải pháp clorua...
  • 4
  • 347
  • 0
Báo cáo y học:

Báo cáo y học: "IV among pregnant women in Moshi Tanzania: the role of sexual behavior, male partner characteristics and sexually transmitted infections" pot

... problem among women of reproductive age The behavior and other characteristics of the male partners in this study were important predictors for HIV in women Therefore, involvement of men in HIV ... encouraged to inform their partners and bring them for counseling and testing, and those with proven sexually transmitted infections were given a contact card to give to their partners so that they could ... treatment All the services were free of charge for both the women and their partners At the time the study was conducted, there was no routine service for counseling and testing of pregnant women for...
  • 10
  • 430
  • 0
The role of paxillin superfamily members  hic 5 and leupaxin in b cell antigen receptor signaling 1

The role of paxillin superfamily members hic 5 and leupaxin in b cell antigen receptor signaling 1

... membrane fraction 45 < /b> 46 47 47 50< /b> 50< /b> 51 52< /b> 53< /b> 54< /b> 55< /b> 55< /b> 56< /b> 56< /b> 57< /b> 58< /b> 58< /b> 59< /b> 59< /b> 59< /b> 60 61 62 62 62 62 63 63 64 65 < /b> 65 < /b> 66 67 68 CHAPTER 3: THE < /b> ROLE < /b> OF < /b> HIC-< /b> 5 < /b> IN < /b> B CELL RECEPTOR SIGNALING 3 .1 Introduction 3.2 ... Ligases 1. 6.4 .1 C-Cbl 1. 6.4.2 Cbl -b Paxillin < /b> superfamily < /b> members < /b> 1. 7 .1 Paxillin < /b> 1. 7.2 Hic-< /b> 5 < /b> 1. 7.3 Leupaxin < /b> Rationale and < /b> aims of < /b> this project 1 10 12 13 17 20 23 26 26 26 28 29 29 31 32 32 33 35 < /b> 35 < /b> ... 3 .5 < /b> 3.2.4 Interaction of < /b> Bam32 homologues: TAPP1 and < /b> TAPP2, with Hic-< /b> 5 < /b> and < /b> paxillin < /b> 75 < /b> 3.2 .5 < /b> PH domain of < /b> Bam32 mediates binding to Hic-< /b> 5 < /b> and < /b> paxillin < /b> 78 3.2.6 Interaction of < /b> Hic-< /b> 5 < /b> and < /b> paxillin...
  • 191
  • 553
  • 0
The role of paxillin superfamily members  hic 5 and leupaxin in b cell antigen receptor signaling 2

The role of paxillin superfamily members hic 5 and leupaxin in b cell antigen receptor signaling 2

... Thus, leupaxin < /b> plays an inhibitory role < /b> in < /b> BCR signaling and < /b> B cell function Inhibitory Role < /b> of < /b> Leupaxin < /b> in < /b> BCR Signaling RESULTS Leupaxin < /b> Is Activated upon BCR Engagement in < /b> Human BJAB B Cells—It ... duction of < /b> IL -2 by activated B cells Inhibitory Role < /b> of < /b> Leupaxin < /b> in < /b> BCR Signaling Tyrosine 72 of < /b> Leupaxin < /b> Is Important for Its Inhibitory Function—As shown above (Fig 4B) , Tyr 72 of < /b> LPXN was the < /b> ... Inhibitory Role < /b> of < /b> Leupaxin < /b> in < /b> BCR Signaling 27 184 JOURNAL OF < /b> BIOLOGICAL CHEMISTRY peak between and < /b> 15 < /b> after BCR ligation in < /b> BJAB cells The < /b> binding of < /b> LPXN to Lyn appeared to occur in < /b> response to BCR...
  • 11
  • 334
  • 0
The role of precautionary labelling for food allergens and the care of children with food allergies

The role of precautionary labelling for food allergens and the care of children with food allergies

... labelling in the care of children with food allergies The thesis focuses on two key areas of research The first explores current practices with regard to precautionary labelling and the impact of these ... of the allergic patient 16 General Declaration I, Giovanni Zurzolo, declare that the PhD thesis entitled ‘ The Role of Precautionary Labelling for Food Allergens and the Care of Children with Food ... foods are often used by parents of young children because of their accessibility and ease -of- use Use of processed foods is more complicated for parents of children with food allergy because of...
  • 135
  • 394
  • 0
Tài liệu Báo cáo khoa học: Insights into the interaction of human arginase II with substrate and manganese ions by site-directed mutagenesis and kinetic studies Alteration of substrate specificity by replacement of Asn149 with Asp docx

Tài liệu Báo cáo khoa học: Insights into the interaction of human arginase II with substrate and manganese ions by site-directed mutagenesis and kinetic studies Alteration of substrate specificity by replacement of Asn149 with Asp docx

... considers the 4541 Interaction of arginase II with substrate and manganese ions ´ V Lopez et al Table Kinetic properties of the arginase activities of wild-type and mutant variants of human arginase II ... activity of the Asn14 9Asp variant, it is clear that the interactions of arginase II with l-arginine and agmatine are greatly altered by replacement of this residue with aspartate To the best of our ... mutations on the affinity of metal binding to arginase II To further examine the effects of the His120fiAsn and His145fiAsn mutations on the interaction of the enzyme with manganese ions, maximally...
  • 9
  • 651
  • 0
Báo cáo hóa học:

Báo cáo hóa học: " The impact of spatial correlation on the statistical properties of the capacity of nakagami-m channels with MRC and EGC" pdf

... Rafiq et al.: The impact of spatial correlation on the statistical properties of the capacity of nakagami-m channels with MRC and EGC EURASIP Journal on Wireless Communications and Networking ... used to find the statistical properties of the channel capacity 3.1 Statistical properties of the capacity of spatially correlated Nakagami-m channels with MRC The PDF p g (z) of the instantaneous ... presents the derivation and analysis of the PDF, CDF, LCR, and ADF of the instantaneous channel capacityc of spatially correlated Nakagami-m channels, for both MRC and EGC The PDF of the channel capacity...
  • 12
  • 606
  • 0
The Role of Power

The Role of Power

...  Role of Power  Rules for Using Power Role of Power Power defined:  • Ability or official capacity to exercise control;  authority • Ability to influence or control others  Sources of Power ... Relationship between power &  dependence • Power A, B = Dependence B, A • Power of person A over B is equal to the dependence of person B on A Rule #6: Power of Who You Know It’s not what you know but who you know ... Minimally Politicized Arena – power possessed by those  who are truthful and demonstrate regard for their own  outcomes and those of others • Moderately Politicized Area – greater acceptance of behind­ the scenes tactics so long as the goals of the group are ...
  • 20
  • 590
  • 0
 Circuit theory of finance and the role of incentives in financial sector reform

Circuit theory of finance and the role of incentives in financial sector reform

... illustrates the main structural, theoretical and incentive-related policy implications of circuit theory of finance Section I.2 discusses the special role of the financial system as the core of the circuit ... profitability is declining The internalization of information within the same institution may thus enhance intra -circuit and inter -circuit stability by reducing the incentive to overfinancing The ... conceptualization and recent evidence CTF clarifies the role of the financial system in the functioning of a monetary market economy of production At the start of the circuit process, the financial system...
  • 55
  • 665
  • 0
Facts of Vietnam Freight forwarding industry and the role of Vietnam Freight Forwarders Association (VIFFAS) to the industry in international economic integration processhelpful to Oristar.doc

Facts of Vietnam Freight forwarding industry and the role of Vietnam Freight Forwarders Association (VIFFAS) to the industry in international economic integration processhelpful to Oristar.doc

... about the facts of Vietnam freight forwarding industry and the Association s importance to the industry, especially in today’s economic integration process Therefore, I chose the topic Facts of Vietnam ... Association (VIFFAS) and then emphasize on the role of the Association (VIFFAS) to Vietnam freight forwarding industry in international economic integration process, summarize the achievements of the Association ... world The Association has the role of coordinating the activities of the members in order to protect the interests of the members and improve the position of Vietnam in the international freight forwarding...
  • 31
  • 1,229
  • 21
Báo cáo y học:

Báo cáo y học: "Human toxoplasmosis and the role of veterinary clinicians"

... aged This is particularly true with regards to T gondii, where the consequences of infection can be very severe, while the risk of living with one’s beloved cat is practically nill References Angulo ... Shin DW, Lee TY, et al Seroprevalence of Toxoplasma gondii infection and risk factors associated with seropositivity of pregnant women in Korea J Parasitol 2008; 94: 963-965 Grant S and Olsen CW ... 963-965 Grant S and Olsen CW Preventing zoonotic diseases in immunocompromised persons: the role of physicians and veterinarians Emerg Infect Dis 1999; 5: 159-163 http://www.medsci.org ...
  • 2
  • 499
  • 0
The role of language in adult education and poverty reduction in Botswan

The role of language in adult education and poverty reduction in Botswan

... program in Botswana maintains the hegemony and the gap between the poor and the rich, the major and minority groups In order to redress poverty the adult education program needs to be aware of the social ... vital in fighting poverty The adult education program can thus harness the local languages and indigenous knowledge of the minority and poor people and use them to mobilize the poor and minorities ... the learners to be confident to participate in the discussions and activities of their education and economy This involves the teaching of local languages, Setswana and English By involving the...
  • 5
  • 836
  • 1
153 The role of marketing activities to bankcard and actual state of Ngân hàng nông nghiệp và phát triển nông thôn (AgriBank) cards

153 The role of marketing activities to bankcard and actual state of Ngân hàng nông nghiệp và phát triển nông thôn (AgriBank) cards

... continuously made an effort to diversify the variety of services to meet and satisfy better customers’ needs and demands 2.2.3 The role of marketing to Agribank cards Tasks of Marketing Department was ... work and plans of department to the Director, make plans and assign tasks to the staff to complete objects of Department and the branch - Marketing staff: staff are in charge of Card section and ... success of the branch 2.2.2 Current marketing activities The most important function of the department is to research and then bring banking services of the branch to more and more customers Services...
  • 33
  • 662
  • 0

Xem thêm

Từ khóa: the essence of object oriented programming with java and uml pdfthe essence of object oriented programming with java and umlthe role of the usgsthe role of energythe role of capitalthe role of musicthe role of languagethe role of parepistemes in materials sciencethe role of electricalthe role of performancethe role of policy in the fish sectorthe role of fisheriesthe role of antsthe role of rotiferthe role of the courtsNghiên cứu sự biến đổi một số cytokin ở bệnh nhân xơ cứng bì hệ thốngBáo cáo quy trình mua hàng CT CP Công Nghệ NPVchuyên đề điện xoay chiều theo dạngNghiên cứu vật liệu biến hóa (metamaterials) hấp thụ sóng điện tử ở vùng tần số THzGiáo án Sinh học 11 bài 13: Thực hành phát hiện diệp lục và carôtenôitGiáo án Sinh học 11 bài 13: Thực hành phát hiện diệp lục và carôtenôitGiáo án Sinh học 11 bài 13: Thực hành phát hiện diệp lục và carôtenôitGiáo án Sinh học 11 bài 13: Thực hành phát hiện diệp lục và carôtenôitQuản lý hoạt động học tập của học sinh theo hướng phát triển kỹ năng học tập hợp tác tại các trường phổ thông dân tộc bán trú huyện ba chẽ, tỉnh quảng ninhTrả hồ sơ điều tra bổ sung đối với các tội xâm phạm sở hữu có tính chất chiếm đoạt theo pháp luật Tố tụng hình sự Việt Nam từ thực tiễn thành phố Hồ Chí Minh (Luận văn thạc sĩ)Nghiên cứu khả năng đo năng lượng điện bằng hệ thu thập dữ liệu 16 kênh DEWE 5000Tìm hiểu công cụ đánh giá hệ thống đảm bảo an toàn hệ thống thông tinChuong 2 nhận dạng rui roTổ chức và hoạt động của Phòng Tư pháp từ thực tiễn tỉnh Phú Thọ (Luận văn thạc sĩ)Kiểm sát việc giải quyết tố giác, tin báo về tội phạm và kiến nghị khởi tố theo pháp luật tố tụng hình sự Việt Nam từ thực tiễn tỉnh Bình Định (Luận văn thạc sĩ)Giáo án Sinh học 11 bài 15: Tiêu hóa ở động vậtchuong 1 tong quan quan tri rui roGiáo án Sinh học 11 bài 14: Thực hành phát hiện hô hấp ở thực vậtGiáo án Sinh học 11 bài 14: Thực hành phát hiện hô hấp ở thực vậtĐổi mới quản lý tài chính trong hoạt động khoa học xã hội trường hợp viện hàn lâm khoa học xã hội việt nam