... totheir surface. On the other hand, some of the nanowires aggregated into bundles in the solutionFig. 1. XRD pattern of the as- prepared nanowires (A and Brepresent anatase and brookite, respectively).Fig. ... dif-fraction peak of brookite (denoted as B in Fig. 1)can also be found, it is much lower than those of anatase phase. No characteristic peaks of otherimpurities, such as NaCl and Na2TiO3, ... range (465 and 520 nm band) and attributed them to the oxygen vacancies. Jin et al.[19] observed two peaks at 488 and 510 nm fromanatase TiO2film with the addition of ZnFe2O4 and ascribed...