... 216,72,0 45 8,66,7 (Cu0,2Tl 4, 8Te3) 210,21,7 213,02,2 45 47 (Cu0 ,4 Tl 4, 6Te3) 207,81,6 210,52,3 44 97 (Cu0,6Tl 4, 4Te3) 205,31,6 207,62 ,4 444 8 (Cu0,8Tl 4, 2Te3) ... temperature. At cooling melt crystallizes in fine-grained and microscopic homogeneous state and then annealed at 40 0K for 200 h. Obtained cylindrical ingots in diameter ~8mm cuts like pellets in the thickness ... systematized and critically analyzed in a number of handbooks and monographies [Max Plank Institute, Stuttgart, 1992-1995; M.Babanly et.al, 1993]. Electromotive Force and Measurement in Several Systems...